Witho,

Somewhere in the back of my pea brain I remember someone, I think Sandy King, saying that when double coating, he had to increase his exposure time—could this be an issue with your DMax?

Best Wishes,
Mark Nelson

Precision Digital Negatives - The System
PDNPrint Forum at Yahoo Groups
www.MarkINelsonPhoto.com



In a message dated 1/18/07 10:33:34 AM, info@witho.nl writes:


Yes, it is, 12x20 inch and little sensitizer. That is why I lack some Dmax,
I think, just because I do not use enough sensitizer. I always double coat
with half the strength of the sensitizer. It gives me lots of time to make
very smooth coatings and cope with the hygroscopic effect of the lithium. So
I go to 1.35 with 1 ml metal solution and 1 ml AFO 60% (single coat) or
double coat half the concentrations.

Witho