Re: Taming Fabriano Artistico (Trad. White) for Cyanotype
Hi...
Just thought I'd note that Dick Arenz lists Fabriano New Artistico (which is
the paper I believe you're referring to) as one of the candidates for
acidification as well as double coating, for pt/pd. My guess would be the
same treatment for any iron process...
For my fledgling attempts in argyrotype, acidification proved the key to
making good prints with the EW version.
Paul
----- Original Message -----
From: "Loris Medici" <mail@loris.medici.name>
To: <alt-photo-process-l@usask.ca>
Sent: Tuesday, December 02, 2008 4:51 AM
Subject: Taming Fabriano Artistico (Trad. White) for Cyanotype
I have few questions about Fabriano Artistico Trad. White & Trad.
Cyanotype:
Is there anyone using this paper for Trad. Cyanotype? Do you pre-treat the
paper before printing Cyanotype?
I had a bad experience with Fabriano Artistico and New Cyanotype,
therefore plan to acidify (or neutralize) the paper before printing Trad.
Cyanotype. I remember someone's nice Cyanotype prints on Artistico but I'm
not sure if it was the Trad. White or Extra White variant.
I want a paper which is good for both Cyanotype and Gum -> I want for more
dmax / punch with my color prints, therefore want to use Cyanotype as the
Cyan layer.
BTW, any non staining / transparent M and Y primary pigment suggestions
would be highly appreciated. As far as I can see, Schmincke PV19 is nice
as Magenta but PY151 of the same brand has too much filler and kills the
underlying layers by seriosly clouding them (despite being marketed as
semi-transparent)...
I plan to:
1. mix 0.5M (~50ml 35% HCl into water givin a final volume of 1000ml) HCl
and
2. put the paper into it for not more than 10 minutes and
3. transfer the paper into salted water (to suck the HCl out of the paper
by osmosis) few minutes
4. rinse it (flushing several times) in pH neutral tap water
Do you think the above procedure is fine to get rid of the calcium
carbonate buffer in the paper w/o disturbing it's integrity?
Should I lightly size the paper after acid treatment in order to get a
decent (contrasty and sharp) Cyanotype layer of will it work OK?
Thanks in advance!
Loris.
P.S. I know I can try this and see for myself but I'm sure there are
people already tried this before, so I'm trying to save time by not
pursuing an lenghty but equally ineffective(?) procedure...