U of S | Mailing List Archive | alt-photo-process-l | Re: PtPd double coating on COT 32?

Re: PtPd double coating on COT 32?


  • To: alt-photo-process-l@usask.ca
  • Subject: Re: PtPd double coating on COT 32?
  • From: Philippe Ayral <payral@gmail.com>
  • Date: Mon, 01 Jun 2009 14:15:06 +0200
  • Comments: "alt-photo-process mailing list"
  • Delivered-to: alt-photo-process-l-archive@www.usask.ca
  • Dkim-signature: v=1; a=rsa-sha256; c=relaxed/relaxed; d=gmail.com;s=gamma; h=domainkey-signature:mime-version:received:in-reply-to:references:date:message-id:subject:from:to:content-type;bh=ThtooKvxdOsm0RUPAbF9nNvvpeA5MrlRBcNWokYJa5A=;b=G4sUON1MsIv+tnehxjXw5zOQOAX+VBc8QCWvjjEqQbdQWno/mkjmH65tGE13itL18GSyMdTIARC6h9Js4snMHzlkt4XTm3sO0sNIT6OmL2pIL6vhZSs/h3VmLBzxjgiGw7BKCj6fYt27TwZ5wSBrbMx/Pe60TVIUkX9qiIV/eZM=
  • Domainkey-signature: a=rsa-sha1; c=nofws; d=gmail.com; s=gamma;h=mime-version:in-reply-to:references:date:message-id:subject:from:to:content-type;b=WDChgPcxLMghFRFvYX49KsF/UQsgdKXbryCx6sdukSWARVMDuOEEcACFGcHPiorPXpIBzXo05AvXLuiYzyUK3KzyiCTUzaKI2ebtPGMj95NitkJBVR2KAkLwvGQYWPdeW/gbJdNmTm4dSvQNSRX5GoBki/0GTnfVokcCpZdgms8=
  • In-reply-to: <4A23C407.9070209@jacquesverschuren.nl>
  • List-id: alt-photo-process mailing list <alt-photo-process-l@sask.usask.ca>
  • References: <901983.78185.qm@web27803.mail.ukl.yahoo.com><9527a22e0905251031h16ad88f9v74f27a76e546ff3c@mail.gmail.com><899366.24413.qm@web27806.mail.ukl.yahoo.com><9527a22e0905261040w78d1f8cey7ff0e6b31a12abd0@mail.gmail.com><000601c9df0b$27f80610$7000a8c0@dell4600><49492.85.99.254.37.1243458276.squirrel@loris.medici.name><000301c9df15$26b197d0$7000a8c0@dell4600><23023.62.244.225.182.1243491799.squirrel@loris.medici.name><5C11A9EEE1FD4AD2AE932493C74C7B9E@daubasi38bqsf8><4A23C407.9070209@jacquesverschuren.nl>
  • Reply-to: alt-photo-process-l@usask.ca

No. COT 320 doesn't need double coating. The only need is warmth (> 20° C) and high humidity level (> 50%).


2009/6/1 Jacques Verschuren <info@jacquesverschuren.nl>

Would COT 32 seriously benefit from double coating for Ptpd printing? If so, what would the best way be to proceed (dilution, etc.)?