[alt-photo] Re: Gum over cyanotype question
Willen, Matthew S
willenm at etown.edu
Mon Feb 27 17:23:14 GMT 2012
Yes, with gel/glut. Maybe it's to give it shot unsized. M
On 2/27/12 12:07 PM, "Henry Rattle" <henry.rattle at ntlworld.com> wrote:
>Matt - is your FA HP sized before the first coat? I sized with
>gelatin/formaldehyde before starting, and found this paper got pretty
>slick
>after a coat or two.
>
>Henry
>
>
>On 27/02/2012 16:21, "Willen, Matthew S" <willenm at etown.edu> wrote:
>
>> Hi Francis
>> Fabriano Hot Press extra white, 300 lbs
>> Potassium, 1 part gum, part mixed gum/pigment, 2 parts Na dichromate
>> Gum exposure about 8 minutes under a bank of 12 uvbl bulbs.
>>
>> --Matt
>>
>> On 2/27/12 10:57 AM, "francis schanberger" <frangst at gmail.com> wrote:
>>
>>> These will probably help the discussion:
>>>
>>> What paper are you using?
>>> What is the gum sensitizer mixture? (ammonium or potassium dichromate)
>>> (1:1
>>> or ?)
>>> How long is your gum exposure?
>>>
>>> -francis
>>>
>>>
>>> --
>>> francis schanberger
>>>
>>> www.francisschanberger.com
>>> _______________________________________________
>>> Alt-photo-process-list | http://altphotolist.org/listinfo
>>
>> _______________________________________________
>> Alt-photo-process-list | http://altphotolist.org/listinfo
>
>
>_______________________________________________
>Alt-photo-process-list | http://altphotolist.org/listinfo
More information about the Alt-photo-process-list