On 18 apr. 2013, at 05:05, Greg Mikol <greg.mikol at ieee.org> wrote:
> Kees...what is the wet thickness of your tissues?
For small formats (~a4) I make fairly thick tissues @1mm wet thickness. Larger formats I am coating with a #200 coating rod that lays down a 0,47mm wet layer.
I never had problems with nitrogen release resulting in bubbles, white spots or other problems.
kees