I do citric acid followed by 2 baths of hypo mixed with EDTA. Watch out that your water bath is acidic - if it's basic it can lock in the ferric. That's why I go straight from the pot ox to citric acid.
Jeremy
Sent from a mobile device.
> On Nov 5, 2013, at 12:02 PM, Doug Taylor <dougtaylor13 at mac.com> wrote:
>
> Hi Diana,
>
> Appreciate you sharing your clearing technique.
> My current clearing technique may be overkill, not sure, as it was an approach I had read a while ago. But definitely going to give you approach a try, as it's simpler and cheaper! I'm all for simple and saving money if it works.
>
> Thanks again for sharing, Doug
>
>
> On Nov 5, 2013, at 12:46 PM, Diana Bloomfield wrote:
>
> Hi Doug,
>
> I use only water and citric acid/water for clearing baths. I do a running wash at the end as well. For Revere, that seems to work fine for me. I hate to keep harping on COT320, because Bob likes it and obviously has no problem-- and I'm sure other people do as well-- but that is the one paper that I had a heck of a time clearing. Maybe it's my water over here. But with both Arches and with the Revere, water baths and citric acid/water baths seem to be fine for clearing. But I'm sure what you're doing now would work as well-- seems a little overkill-- but if it works for you . . . :)
>
> Diana
>
>> Hi Diana,
>>
>> As I mentioned earlier, I've been using Fabriano Artistico EW Hot Press to print pt/pd, and I was acidifying with Oxalic acid prior to coating and printing.
>>
>> You mentioned using Arches, COT320, and Revere without acidifying these papers. I have the Revere which I am going to use shortly.
>>
>> Wonder what your clearing process is with these papers, after development?
>>
>> With the Fabriano, after development, I let the print sit in a tray of water for 5 minutes, and then 3 successive baths of 5 minutes each; 1) 2% citric acid 2) Kodak hypo clear with a TBS of EDTA Tetrasodium per liter, 3) another tray of Kodak hypo clear with EDTA, and finally a wash in running water for 20 minutes.
>>
>> Would this clearing process work with the Revere paper or do you prefer another process?
>>
>> Thanks, Doug
>
> _______________________________________________
> Alt-photo-process-list | altphotolist.org
>
> _______________________________________________
> Alt-photo-process-list | altphotolist.org
_______________________________________________
Alt-photo-process-list | altphotolist.org
More information about the Alt-photo-process-list
mailing list