Mark,
Twenn 20 could be used on Cot 320 but at really high dilution such like 1
drop of 1% or 0.5% for an 8x10, if used at 5 or 10 % the paper change to
sponge.
Dan
I prefer to humidify the paper before coating.
The I coat the paper, and let it dry without warm or any air spread on it. I
store it 10 minutes , then dry it a ittle and expose. double coating may
help getting denser black but it also modify the curve of the sensitizer, I
truely prefer to make an heavier single coat , I don't find that acid oxalic
add any density or quality to this paper.
Cot 320 is a litlle like Arches platine and it is a really tough paper ( not
like Cranes or some vellum), when you coat it you can press a little more
the coating rod or your brush. you can brush for longer and cot rod till
there is no more line.
a little
Amicalement
best regards
Nzé Christian
mailto:christian_nze@hotmail.com
http://www.c-nze.com
_________________________________________________________________
MSN Messenger http://g.msn.fr/FR1001/866 : un logiciel gratuit pour
dialoguer avec vos amis !
Received on Sun Feb 29 17:46:16 2004
This archive was generated by hypermail 2.1.8 : 04/01/04-02:02:04 PM Z CST