Oxalic Acid for Pt./Pd.

From: Sandy King ^lt;sanking@clemson.edu>
Date: 09/15/04-10:02:28 AM Z
Message-id: <a06020404bd6e16c188d6@[192.168.2.2]>

I get higher Dmax by about 0.10 - 0.20 with most papers in Pt/Pd.
printing by first soaking in a 1% solution of oxalic acid, then
drying without rinsing.

Soaking papers this way is not terribly inconvenient, but I am
wondering if anyone has experimented with adding oxalic acid directly
to the sensitizer before coating?

Sandy King
Received on Wed Sep 15 10:02:42 2004