On Sat, 12 Mar 2005, Christina Z. Anderson wrote:
>>
>> Could it be that putting the hardener IN the gelatin makes a/the
>> difference? Or -- were these spray developed??? Maybe spray development is
>> *better* with boiled ?
>> Judy
>
> I do put the hardener in the gelatin. I do use glut. I brush on my
> hardener. This is on Fabriano Artistico EW hot press and cold TW.
I've tested formaldehyde against glyoxal, but never tested either of them
against glut -- Maybe the glut could protect the size in some way against
the ravages of scalding water...?
A thought, anyway....
Judy
Received on Mon Mar 14 00:41:41 2005