Rajul,

>
I have tried pre-coating w oxalic acid - it produced an
unacceptable increase the density of blacks but no relief from clearing
problems w BFK.
>

I'm not sure if I'm understanding correctly, but I meant pre-soaking, not
pre-coating. Try a 2% solution of oxalic soaked for 20 minutes.

Clear in 3-5% citric acid.