polymer plate drying time
Hi all, Back to some basics here... I think some of my uneven tone problems are coming from minerals in our water leaving deposits (we have very hard water from a mountainside well). So... I'm now trying distilled water for washing, but I'm wondering about if I've been drying the plates long enough, with just a few moments under a warm blow dryer, then a 200 sec 1000w hardening exposure. Jon I just went back to your process notes and see that you're doing 600 sec at 1000, but no mention of drying time. comments and suggestions gladly accepted :o) Susan -- susan gravure blog at www.susanvossgravures.blogspot.com website www.dalyvoss.com
|