[alt-photo] Re: About PVA sizing...

Loris Medici mail at loris.medici.name
Tue Nov 22 13:41:40 GMT 2011


Yes, dichromate is (at least) non-volatile while some hardening agents are extremely volatile. (I remember experiencing headache after sizing sessions, occasionally - even I was using very little formalin; a few milliliters into 100ml sizing solution...)

Regards,
Loris.


-----Original Message-----
From: alt-photo-process-list-bounces at lists.altphotolist.org [mailto:alt-photo-process-list-bounces at lists.altphotolist.org] On Behalf Of Diana Bloomfield
Sent: 22 Kasım 2011 Salı 15:33
To: The alternative photographic processes mailing list
Subject: [alt-photo] Re: About PVA sizing...

Yes, I think the non-toxicity (as opposed to glutaraldehyde or
glyoxal) factor is worth it.  Still using dichromates, of course, but eliminating other toxic elements is always a good thing.