Pyro
KOUKLIS, KERIK T (Kerik.Kouklis@Aerojet.com)
Fri, 10 Oct 1997 11:04:16 -0700
I use PMK Pyro with FP4+, Tri-X, and HP5+ (in order of preference) for
virtually all of my platinum/palladium work. It produces a wonderful
scale for this process, although exposure times are extended somewhat
due to the yellow-green stain produced by this developer. My average
exposure times are 10 to 15 minutes in a 40 watt UV flourescent box. A
side benefit is that the negatives are still very appropriate for
printing on soft gelatin silver papers.
Kerik Kouklis
http://www.jps.net/kerik/