I have found two things that seem to help even the staining on TMX. I use
one drop of Edwal LFN/300ml of working developer, I'm not sure that it does
anything but it make me feel better. The other thing which I know makes a
differance is to wash the developing reels in almost hot water after use to
remove the Photoflo. You did not say, did you add EDTA to your stock? If
not you should also add EDTA if you are using a Jobo.
ken hatch
http://home.swbell.net/khatch1
-----Original Message-----
From: Herold Faulkner <faulkner@redshift.com>
To: SCHRAMMR@WLSVAX.WVNET.EDU <SCHRAMMR@WLSVAX.WVNET.EDU>;
alt-photo-process-l@skyway.usask.ca <alt-photo-process-l@skyway.usask.ca>
Date: Monday, January 12, 1998 7:49 PM
Subject: Re: Pyro
>>
>On the subject of PYRO, I am just experimenting with TMX and pyro in my
JOBO
>processor but am having some teething problems. Uneven fog which seems to
>be a result of uneven flow BEHIND the films. Gordon Hutchings has
addressed
>this problem and I expect to have it unnder control one of these days.....
>However, anyone with experience with this is invited to send suggestions.
>
>Thanks,
>
>Hal Faulkner
>
>