potassium chlorate


Dan Koons (dkoons@pld.com)
Mon, 24 May 1999 09:57:13 -0500


I understand some printers use a solution of potassium chlorate for pt/pd
in place of the #2 fo for the develop out printing. what I would like to
know is if there is a chart for how much to use. for example what would one
use in a formula that would replace 3 drops #1& 3 drops #2? thankyou dan
koons