Re: Solarizations with Platine and Pt


Gary Miller (gmphotos@earthlink.net)
Wed, 28 Jul 1999 10:39:35 -0700


Jeff;

The contrasting agent that I am using is the typical solution number 2 from
B&S;

ferric oxalate 6.5 g
potassium chlorate 0.33 g
water to make 25 ml

While it was mentioned by Jan, about how much the sensitizer soaks into the
paper, what is the general opinion on how long to let the sensitizer soak
into the paper, Platine for example, after coating and before drying.

Gary