Re: Maintaining contact.

From: fishy (fishy@mediaone.net)
Date: Tue Dec 21 1999 - 21:30:12 /etc/localtime


Darlington Media Group wrote:
>
> Dear list,
>
> Help! I'm having trouble with small 'soft spots' on printing 20x8 inch
> pd/pt prints. I'm sandwiching the negative and sensitised paper
> (Arches
> platine) between two sheets of quarter plate glass and using the
> traditional pd develop out process ie. the paper is dry.
>
> Would a thin sheet of foam or rubber under the negative help? How
> about
> edge clips?
>
> I would be delighted to hear from anyone who has experience in this
> area.
>
> Thanks ..... Tony McLean.

Dear Tony-

You can try a thin layer of neoprene (it may also be called closed cell
foam). I believe it's the type used for diver's wet suits. About 1/8th
inch thick.

Best,
Dan Donovan



This archive was generated by hypermail 2b29 : Tue Jan 11 2000 - 12:10:49