Dear list,
Help! I'm having trouble with small 'soft spots' on printing 20x8 inch
pd/pt prints. I'm sandwiching the negative and sensitised paper (Arches
platine) between two sheets of quarter plate glass and using the
traditional pd develop out process ie. the paper is dry.
Would a thin sheet of foam or rubber under the negative help? How about
edge clips?
I would be delighted to hear from anyone who has experience in this area.
Thanks ..... Tony McLean.