Bob,

That's very interesting. Could heat drying cyanotype sheets make them
enough lower in contrast to print platinum negs? It's a good
possibility. Even doubling the B solution of cyano doesn't get the stuff
anywhere near soft enough to print my Pt negs, but if heat drying can
*consistently* lower the contrast that would be great.---Carl

-- 