From: Kerik Kouklis (Kerik@Kerik.com)
Date: 01/05/03-10:26:15 PM Z


Sandy,

I suggest a 5 min. soak with Uno rather than a dip and dunk. I use 1% OA
with this paper (although I think 2% would also be fine). I presume your 20%
is a typo... I discard the OA solution rather than save it. OA is dirt
cheap.

Kerik

> I may try the 20% oxalic acid treatment with Fabriano Uno for
> kallitype since this paper is so well sized and gives great results
> with VDB. How long is the dunk, and can you re-use the oxalic acid
> solution or do you use it and discard?
>
> Sandy