Ray, if you are looking into processing "Lipps", you might consider those:

GP-3
stock solution:
phenidone.................0.2g
hydroquinone...............5g
sodium sulfite...........100g
potassium hydroxide..25g
amonium thiocyanate..45g

15ml stock solution + 400ml distilled water: 5 - 15min. at 20°C

Valenta
A
pyrogallol.................1g
water......................100ml

B
ammonia (s.w. 0.91)..67ml
potassium bromide......20g
water......................200ml

10ml A + 20ml B + 70ml water

Generally speaking of that kind of developers (= "colloidal developers")
developing times might greatly depend on the initial emulsion hardness as
well as silver concentration and grain size...

Martin

----- Original Message -----
From: "Bill William" <iodideshi@yahoo.co.jp>
To: <alt-photo-process-l@sask.usask.ca>
Sent: Tuesday, August 24, 2004 6:29 AM
Subject: physical developers

> Speaking of physical developers, anyone here use them?
>
> Got any formulas / experience you would like to share?
>
> Ray
>
> __________________________________________________
> GANBARE! NIPPON!
> Yahoo! JAPAN JOC OFFICIAL INTERNET PORTAL SITE
> http://mail.ganbare-nippon.yahoo.co.jp/
>
Received on Tue Aug 24 04:05:34 2004

This archive was generated by hypermail 2.1.8 : 09/14/04-09:18:00 AM Z CST