Jim,
My experience is that palladium based processes (both develop and printout
type)don't gain anything by letting the Pd mixture sit around, although my
Ziatype mix is a variant, not an exact recipe.
Marek, Houston

> I was reading in one of the online FAQ's that after mixing the platinum
> with the Ferric oxalate, you should let it sit for an hour before
> coating. I'm currently working with Ziatypes.. is this necessary for
> this process as well? Since I haven't been doing this, what gains should
> I see?
>
> Thanks
>
> jim
>