Judy,
Those are very nice for first tries--much nicer than my early attempts.
As for brushes, I find that an inexpensive ($2-4) hardware store bristle
brush works better than the foam or the hake. I have not mastered glass rod
coating.
I, too, find exposures to be long. With single coated classic
cyanotype 1:1 I need 32 minutes with a digineg and my ink settings. Some of
yours look like they would be better with a longer exposure.
Your POP's are great.
Keep working.