Hello Eric,
I use 3:2:100 PyroCat HD for 10 minutes at 70 degrees in a Jobo - for Bergger
I hope that helps.
Mike
www.ExposeTheShadows.com
Eric Nelson <emanmb@yahoo.com> wrote:
I'm using the data at the Unblinking Eye site data as
a starting point for testing Pyrocat HD and various
films here.
I was wondering if there was a misprint there for
Bergger BPF 200 and I was also wondering what other
folks' times/ratios are for Bergger BPF 200.
On the site on page
for Bergger 200, it calls for a ratio of 2:2:10 for
UV, (in my case platinum/palladium) where most other
ratios listed for other films are 2:2:100. That "0"
makes a big difference!
Any help appreciated.
Eric