Thanks Stane.
 
I think your fixer strenght and fixing time are both are slightly more than what you really need. I fix for 1 minute in 2% fixer. I never experienced bleaching in fixer that way.
 
Regards,
Loris.
 
P.S. I won't leave gold or Pt/Pd toning in favour of selenium-toning, in any circumstance... ;)
 
-----Original Message-----
From: Stane Kocar [mailto:stane.kocar@siol.net]
Sent: 26 Eylül 2006 Salı 09:34
To: alt-photo-process-l@usask.ca
Subject: Re: Selenium-toning Van Dyke Brown prints

... 
After a minute or two of washing I fix for 2 minutes in 5 % hypo following
with final wash for 1 hour. In hypo picure bleaches a little, but after 
...