[alt-photo] Re: Multi coat Gum -3rd+ coats tends to wash off

John Brewer john at johnbrewerphotography.com
Wed Mar 3 11:25:39 GMT 2010


Hi Peter,

I'm glad you have solved your adhesion problem. Maybe put down a couple of
layers to get the pigment saturation you are after?

> I still have no understanding as to why there were no problems with 
>these thick layers when laying down the cyan layer first.

Another idiosyncrasy of gum I guess.

Best wishes,

John.


-----Original Message-----
From: alt-photo-process-list-bounces at lists.altphotolist.org
[mailto:alt-photo-process-list-bounces at lists.altphotolist.org] On Behalf Of
pfriedrichsen at sympatico.ca
Sent: Tuesday, March 02, 2010 10:31 PM
To: The alternative photographic processes mailing list
Subject: [alt-photo] Re: Multi coat Gum -3rd+ coats tends to wash off

Loris et al,

I was attempting to produce very saturated layers and in that 
attempt, I increased the gum concentration in order to accommodate 
(without staining), the amount of pigment that was required. Once I 
reduced the gum and pigment concentration, the adhesion was improved 
and the top layer behaved.

I still have no understanding as to why there were no problems with 
these thick layers when laying down the cyan layer first.

Thanks to all for the assistance.

Peter




No virus found in this outgoing message.
Checked by AVG - www.avg.com 
Version: 9.0.730 / Virus Database: 271.1.1/2714 - Release Date: 03/02/10
19:34:00
-------------- next part --------------

No virus found in this outgoing message.
Checked by AVG - www.avg.com 
Version: 9.0.730 / Virus Database: 271.1.1/2719 - Release Date: 03/02/10 19:34:00


More information about the Alt-photo-process-list mailing list