No. As it works well for me I didn't try anything else.
I use citric acid alone when I print on Crane Cover. (not made any more)
2012/2/24 Loris Medici <mail at loris.medici.name>:
> Thanks Philippe!
>
> Out of curiosity, I found a formula that says:
>
> 2 Tbsp Na4.EDTA
> 1 Tbsp citric acid
> 1 Tbsp sodium sulfite
>
> The EDTA:sulfite proportions are reversed here, I guess it's not
> critical - as long as they're together. Do you have any experience
> with a formula similar to the above?
>
> Regards,
> Loris.
>
>
> 23 Şubat 2012 14:36 tarihinde Philippe Ayral <payral at gmail.com> yazdı:
>> In my work I use 20g sodium sulfite per liter (should be a heaping
>> dessert spoon) plus a half one for EDTA.
>> It works for Arche Platine.
>>
>> 2012/2/23 Loris Medici <mail at loris.medici.name>:
>>> Anyone with a quick kitchen formula for sodium sulfite + tetrasodium
>>> EDTA clearing bath for pt/pd? (I mean something like: 2 dessert spoon
>>> sulfite + 2 dessert spoon EDTA into 1000ml water...)
> _______________________________________________
> Alt-photo-process-list | http://altphotolist.org/listinfo
--
Philippe Ayral
http://payral.pagesperso-orange.fr