[Alt-photo] Re: casein prints

Jorj Bauer jorj at jorj.org
Wed May 29 02:05:54 UTC 2013


> Glass is new to me. I was thinking of getting Yupo, but certainly will try casein on glass. I have a bunch of very thick glasses, no fear that they get broken. What about sheets of plastic? Will they serve equally as a smooth surface? Much easier to cut than glass. Also brushing until dry is new, I've used a foam roller and get quite smooth coating (trick from Alex Charter's tempera guide).

I've worked with carbon on Yupo, but not casein on Yupo (yet). I can say that plexiglass is *not* a good choice for casein - the one day that I tried working with plexi, the casein slid off during development no matter what I did to prep the surface.

-- Jorj



More information about the Alt-photo-process-list mailing list