kallitypie fixer

marc bruhat (sillage@magic.fr)
Wed, 19 Feb 1997 14:12:59 +0000 (GMT)

I use a system particular for make some kallitypie:
I coat with ammonium ferric oxalat and I develop in a bath of silver nitrate
(2%).
I have tried to fix in the chloridric(?) acid, in hyposulfit and in the
sodium sulfit; the yellow bottom remains always.
Nobody ruled this &"%¤}@ problem?
Thank you
marc bruhat