From: Witho Worms en Jorien van Santen (verzet13@xs4all.nl)
Date: 10/08/01-08:48:52 AM Z
I'm busy doing double transfer carbon printing. Until now I am getting each
time marks from, I guess, separating the tissue from the plexi (wave like
patterns as the sea leaves on a beach). Before developing I give the plexi
with tissues a 10 minute rest and after that a 2 minute alcohol dip. How can
I avoid these marks.
I have separated tissue and plexi after two minutes but also after 4 minutes
of development in 40-42 Celsius. In both cases I had the marks.