From: clay (wcharmon@wt.net)
Date: 01/14/02-05:12:25 PM Z
WHAT! Make it easier!
----------
>From: Kerik717@aol.com
>To: alt-photo-process-l@skyway.usask.ca
>Subject: Re: Papers
>Date: Mon, Jan 14, 2002, 4:20 PM
>
>Carl, Clay, etc.
>
>Another way to do this is a quick dip and dunk in a tray of 1% oxalic. You
>can batch treat a whole bunch of paper this way much quicker than brush or
>rod coating each sheet. I like to do this with BFK because I sometimes
>print on the front (more texture) and sometimes print on the back (smoother
>surface). One quick dip, then hang to dry and both sides are treated.
>
>Kerik
>
>> Coat with 1% oxalic, let dry, then coat with metal+sensitizer. I think it
>> helps Platine with smoothness of tone and warmth of tone as well.
>>
>> Clay
>
>
>
This archive was generated by hypermail 2b30 : 02/15/02-11:47:41 AM Z CST