--- Ryuji Suzuki <rs@silvergrain.org> wrote:
"For example, cross links formed with formaldehyde... are
not very stable, and they can be broken with weak acid or
high temperature."
Where did you read that?
I do not recall formaldehyde cross links being so fragile
as you claim.
I belive well formaldehyde hardened gelatin can (in a
sense) withstand boiling.
???
Ray
__________________________________________________
Do You Yahoo!?
Yahoo! BB is Broadband by Yahoo!
http://bb.yahoo.co.jp/