Whatman, Fabriano Artistico and Rives BFK do NOT need additional sizing
after oxalic acid treatment.
Kerik
www.kerik.com
> -----Original Message-----
> From: Eric Neilsen [mailto:e.neilsen@worldnet.att.net]
> Sent: Tuesday, May 30, 2006 3:39 PM
> To: alt-photo-process-l@usask.ca
> Subject: RE: Platinum/Palladium & Paper Speed
>
> I had an old supply of Stonehenge natural that since it was
> no longer working for PT/PD I thought it might be a good
> choice. I must certainly was worse after the acid soak. I
> don't know what it was sized with.
>
> I also ran a test on Coventry Rag and it also failed without
> an additional gelatin coating.
>
> There maybe others I am forgetting now.
>