Domenick Mirando (DOMM@delphi.com)
Sat, 13 Feb 1999 18:14:26 -0500 (EST)
>Chromium like a lot of other heavy metals...such as silver, copper, etc
>...can fairly easily [and with very simple equipment] be electroplated
>out of solution and sold or more easily disposed of through means such
>as public haz mat disposal programs...I am sure someone out there is
>doing mixed metals plating out -- bob
In the way that I'm set up now, a large catch sink drains into the plastic
bucket, which empties when full as necessary. I don't keep any standing
quantity of water/chemicals except for the bucket.
I suppose that I could add the sodium sulfite to the bucket if I go *slow*
and use little water to rinse, but it fills quickly...
...one question I have would be...how long must the waste water and
neutralizer set? (Hal?) Does this happen as soon as mixed?
Realtime-electroplating on the fly would pose some interesting physic
problems. <G>
---Dom
This archive was generated by hypermail 2.0b3 on Sat Nov 06 1999 - 10:06:50