stefan@2s-image.de
Date: 01/08/01-02:10:44 AM Z
Hi everybody,
I wonna try now again the Gelabrom process (very
closed to Carbro) but have only ammonium dichromate
as I use it for carbon transfer.
Can I use the ammonium dichromate for a potassium
based formula and how should I alter the ammount
(as ammonium dichromate should react more heavily
as the potassium version does)?
The original formula is:
Potassium ferricyanide 4,0 g
Potassium dicromate 3,0 g
Potassium bromide 2,0 g
Succinic acid 1,1 g
Potassium alaun 0,5 g
Distilled water 250 ml
Thanks to the chemical experts on the list
& best Regards!
Stefan
This archive was generated by hypermail 2b30 : 02/05/01-11:45:21 AM Z CST