Ok, things become clear now... Thank you very much for reminding Clay's
article!
What do you think about including a trace amnt. of 1% oxalic acid into
sensitizer? (for instance: 1 drop = 0.05ml to 1ml sensitizer)
It seems that PH of paper and/or developer/washing water is very important
in Pt/Pd printing... It seems that I have to seriously study this issue.
Thanks,
Loris.
----- Original Message -----
From: "Don Bryant" <dstevenbryant@mindspring.com>
To: <alt-photo-process-l@sask.usask.ca>
Sent: Tuesday, October 12, 2004 12:28 AM
Subject: RE: Another Ziatype question
Loris and Christian,
Although I've never used Whatman HP, Clay Harmon writes in his article about
Gum over Platinum, that Whatman HP should be treated to a 1.5% oxalic soak
to prepare for palladium printing. I assume that may hold true for ziatype
printing as well with that paper.
Don Bryant
Received on Mon Oct 11 15:46:18 2004