As we know a pre-soak in a 1-2% solution of oxalic acid can add quite
a bit of Dmax in Pt./Pd. printing with some papers. Does anyone know
the mechanism of how this works? Is it merely a question of
acidifying the paper? Has anyone ever compared the results between
papers pre-soaked in oxalic acid and in some other dilute acid
solution, say a 1-2% solution of citric acid?