Re : Re: grooves on tubes RE: jobo help


Jcpronier@aol.com
Mon, 25 Oct 1999 02:04:41 -0400 (EDT)


I got the problem with the antihalation layer, using BF200 Bergger 8/10 film
in my jobo cpe2+.
Due to contact with the forms inner the tube, I got straigth lines where the
antihalation layer was not totally removed. I thought it was not a big
problem, and just needed to end process plunging the film in a tray for
additionnal fixing then antihalation complete removing.
This work fine developing in HC110 bath, but with the PMK, the tint due to
metaborate is not even and less tinted on these famous lines without
possibility to solve the pb. So I'm wondering to modify the inner jobo tube
to prevent contact . May be I'll be obliged to developp only one 8/10 sheet
(intead of two), due to internal diameter reduction resulting with spacers.