Re: Gum or what?

Date view Thread view Subject view Author view

From: Judy Seigel (jseigel@panix.com)
Date: 02/20/02-12:18:42 AM Z


On Sun, 17 Feb 2002 Grafist@aol.com wrote:

> > That *two percent* dichromate solution is amazing. Did you really do 2%?

> Yes! ! .I have also used 0.0625% and upwards with good results. I keep
> solutions of different strengths of Ammonium Dichromate as I usually
> sensitize by dunking the dried coated paper rather than brushing on
> sensitized solutions .
> ............................................................
> I used 2%, not by calculation but by hit and miss. I didnt mention the
> ammount of dichro solution. It must have been about 100 ml then mixed with a
> few squirts of paint. Why not try it?

Well, by my calculations, if the volume of "dichro" was so much greater
than the paint (a few "squirts"), say about 10 times as much (?), that
means in effect you had a 20% solution -- wouldn't you say????

And if so, it doesn't count as 2%...

However, you don't say how far from the light source that 15 minutes
exposure was... Also a factor in actual exposure...

> 15 minutes but increased to 25 minutes for subsequent print using same prep
> as first)