My two cents too: As I print quite only Palladium I had sometimes some
bronzing on the sides where there was more coating deposed (I used only
puddle pusher to coat). Now I use a coating road to start ( a quick back
& forth to cover the surface and again two passes with strength) the
coating and a brush just after to finish the job and from that I got a
deeper black (better D-Max) and no more bronzing.
In my lab RH is always between 45 and 65 %.

-- 